NON-ALLOY LOW CARBON STEEL
NORM: PN-EN 10025
APPLICATION:
Steel susceptible to construction steel structures, welding, riveting and bolted structures working at the ambient temperature.
TECHNOLOGICAL INFORMATION:
Fully killed steel; weldable steel
SEMI-FINISHED PRODUCTS:
Fully killed steel; weldable steel
CHEMICAL COMPOSITION:
| C | Mn | Si | P | S | Cr | Ni | Mo | V | Nb | Ti | Al | Cu |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Max 0,20 | Max 1,60 | Max 0,55 | Max 0,025 | Max 0,025 | - | - | - | - | - | - | - | Max 0,55 |
MECHANICAL PROPERTIES:
| Effect of the cross-section on mechanical properties | ||||||||||||
| Ultimate tensile strength | ||||||||||||
| Thickness, mm | < 3 | > 3–100 | > 100–150 | > 150–250 | ||||||||
| Rm, MPa | 510–680 | 470–630 | 450–600 | 450–600 | ||||||||
| Yield stress | ||||||||||||
| Thickness, mm | ≤ 16 | > 16–40 | > 40–63 | > 63–80 | > 80–100 | > 100–150 | > 150–200 | > 200–250 | ||||
| Re, MPa | ≥ 355 | ≥ 345 | ≥ 335 | ≥ 325 | ≥ 315 | ≥ 295 | ≥ 285 | ≥ 275 | ||||
| Elongation | ||||||||||||
| Thickness, mm | ≤ 1 | > 1–1.5 | > 1.5–2 | > 2–2.5 | > 2.5–3 | |||||||
| A80mm, %, longitudinal samples | ≥ 14 | ≥ 15 | ≥ 16 | ≥ 17 | ≥ 18 | |||||||
| A80mm, %, transverse samples | ≥ 12 | ≥ 13 | ≥ 14 | ≥ 15 | ≥ 16 | |||||||
| Thickness, mm | 3-40 | > 40–63 | > 63–100 | > 100–150 | > 150–250 | |||||||
| A, %, longitudinal samples | ≥ 22 | ≥ 21 | ≥ 20 | ≥ 18 | ≥17 | |||||||
| A, %, transverse samples | ≥ 20 | ≥ 19 | ≥ 18 | ≥ 18 | ≥ 17 | |||||||
| Impact test at -20°C | ||||||||||||
| Thickness, mm | > 10–400
27 |
|||||||||||
| KV, J | ||||||||||||
Technological treatment processes:
| Technological treatment processes | Possible application | Temperature, °C | ||
| Hot forming | Forging | + | (1150 – 800) | |
| Rolling | + | (1150 – 800) | ||
| Treatment | Heat treatment | Quenching | – | – |
| Tempering | – | – | ||
| Precipitation strengthening | Supersaturation | – | – | |
| Ageing | – | – | ||
| Annealing | Normalising | + | (890 – 920) | |
| Soft annealing | + | < 580 | ||
| Thermochemical treatment | Carburising | – | – | |
| Other | – | – | ||
INTERNATIONAL STEEL GRADES:
| ISO | EN | Russia | |||
| ~E355-D | ISO 630:1995 | S355J2G3 | EN 10025:1993 | ~17GIS | GOST 19281 – 89 |
| US | Japan | China | |||
| ~A 706 | ASTM A 706 – 00 | ~SM 490 A | JIS G 3106 1995 | ~16Mn | GB T 8164 – 93 |